Cold Weather Bonding

by Don Gutzmer 20 Jun 2021 22:56 PDT
Cold Weather Bonding © Don Gutzmer

During the colder months, the Technical Advisers at West System and ATL Composites are frequently asked "What's the lowest temperature West System Epoxy can be applied?"

Fortunately, it's one they're well equipped to answer. Gougeon Brothers, Inc. got its start in the world of DN Iceboat racing. Both Meade and Jan Gougeon have won multiple DN cup races worldwide. It's not unusual for an iceboat to need repairs mid-regatta, so part of the discipline of iceboat racing is getting epoxy to cure despite cold working environments. The trick is using strategies that bring epoxy temperatures up to adequate cure levels in cold working environments.

Since the 1970s, West System has been using these techniques to assure dependable epoxy bonds throughout frigid Michigan winters. With a little advanced planning, and observing the precautions listed above, you can get West System Epoxy to cure reliably in cold working conditions.

Cold weather techniques

  1. Use West System 105 Resin and 205 Fast Hardener. 205 Fast Hardener is formulated to cure well at temperatures as low as 4 degreesC, but this does require an extended cure time before removing clamps or sanding. 206 Slow Hardener and 207 Special Clear Hardener should not be used below 16 degreesC unless you elevate the working temperature to allow the system to cure properly. For best results when clear coating with 207 Hardener, postpone coating until the temperature in your working environment is around 21 degreesC. 209 Extra Slow Hardener should not be used below 21 degreesC.

  2. Warm resin and hardener before using. Cold temperatures increase the viscosity of the epoxy, making it more difficult to dispense, mix and apply. Warming the resin and hardener lowers their viscosity, allowing the product to flow through the dispensing pumps better, cling less to the containers and mixing equipment, and blend more easily for thorough mixing. The warmer, lower-viscosity mixture will flow more smoothly during application and penetrate porous surfaces more efficiently.

    Methods for warming resin and hardener before use:

    1. Leave the containers in a warm area.
    2. Place a heat lamp near the containers.
    3. Put containers in a cooler with a light bulb or heating pad.
    4. Build a custom warming box out of rigid sheets of foil-backed insulation and keep it warm with a lightbulb or heating pad.
    In any case, you will want the resin and hardener at a temperature between 21 degreesC to 32 degreesC. These methods keep the warmed resin and hardener close to your work and allow less time to cool off between dispensing and application. Warming the epoxy helps the initial chemical reaction get off to a better start, and results in more cross-linking even if the mixture cools when it is applied to a cold substrate.

  3. Dispense resin and hardener at the proper mixing ratio only. Altering the amount of hardener will seriously compromise the epoxy's ultimate strength. WEST SYSTEM 300 Mini Pumps are designed and calibrated to dispense the correct ratio—one full pump stroke of resin for every one full pump stroke of hardener. If you are not able to warm the resin and hardener, do not use excessive force when dispensing. Keep steady pressure on each pump and allow each pump head to make a full stroke down and a full stroke up. Remember, the resin and hardener become thicker and more difficult to pump when they are cold and require significantly more time to return to the top of the stroke.

  4. Stir the resin and hardener thoroughly in a small pot, and allow more time before applying. Mix the resin and hardener for at least two minutes, scraping the sides and bottom of the mixing container. Use a mixing stick shaped to reach the corners of the pot. A smaller diameter mixing pot increases the chemical reaction between resin and hardener because its limited surface area prevents heat from dissipating too quickly.

    If you are unable to pre-warm the resin and hardener, allow some induction time. This simply means letting the mixed resin and hardener stand in the pot for several minutes, then stirring it again before using. This helps get the chemical reaction started, and the exothermic heat the epoxy generates will reduce viscosity making the material easier to apply.

  5. Warm the substrate as much as possible. The epoxy will thin out as it is applied to a warm substrate. It will flow out much more smoothly and penetrate better, resulting in a stronger bond. You can warm a repair area with heat lamps, hair dryers or hot air guns. Small components or materials such as fiberglass cloth can be warmed in a hot box (as described in section 2). Larger areas can be warmed by tenting the area and adding a portable heat source.

    Avoid unvented open-flame heaters that burn kerosene or fuel oil. Unburned hydrocarbons may contaminate bonding surfaces, and elevated moisture and CO2 levels can contribute to the formation of amine blush. Catalytic heaters do not appear to pose a problem unless they are used in a confined space such as an unventilated curing tent or box.

    To prevent temperature-related moisture contamination, be sure you're working in ambient temperatures above the dew point. Your local weather resources will provide the dew point temperature based on relative humidity.

  6. Prepare cured surfaces carefully between applications. When coating at cold temperatures, the slower cure can result in the formation of an amine blush on the surface. The blush feels like a waxy/greasy film on the surface of the cured epoxy. Wash the surface with warm water using a 3-M Scotchbrite™ pad before applying subsequent coatings to a cured surface. Don't let the water evaporate. Dry the surface with plain white paper towels. Sand any remaining glossy areas with medium grit sandpaper.

  7. Allow additional cure time before removing clamps or stressing joints. As a general rule, double the cure time for every 10 degreesC drop in temperature. Allow additional cure more than the 10 degreesC rule for pre-stressed joints, such as bent laminations and joints that will be subject to high loads.

  8. Elevate the temperature of partially cured epoxy. Elevating the temperature of the epoxy after initial cure can help to complete the epoxy mixture's cross-linking and boost the epoxy's physical properties even after a week at cold temperatures. Elevate the temperature of the epoxy and substrate gradually to avoid thermal shock. Although any temperature elevation will improve cross-linking, try to boost the temperature to 22 degreesC or warmer. The time required for final cure depends on the hardener used and the temperature the epoxy is exposed to. Generally, higher temperatures require shorter cure times. Do not exceed 60 degreesC and do not remove clamps or load the joint until the epoxy has cooled.

Caution!

Heating a porous material may cause air within the material to expand and "out-gas". Allow the epoxy to reach a partial cure before elevating the temperature. If an epoxy coating applied over the material has not gelled, bubbles from the out-gassing material may show up in the cured coating or glued joint as it warms. In some cases, your shop will naturally warm itself enough to complete the cure during the day, following a cold night. Outdoors, building a plastic tent to trap heat can easily boost the temperature enough for the epoxy to cure. Turning up the thermostat, using radiant heaters, electric heaters or electric blankets are the most common way to control the cure temperature in a shop. It is not necessary to heat the entire structure if you are working on only a small area. Tents of plastic or insulated board are very helpful for confining heat to specific areas and provide greater mobility with a limited heat source, both indoors and outdoors.

Cold weather storage

It is best to store West System materials above 2 degreesC with the container caps screwed down tightly to avoid moisture contamination. The containers can be stored with the 300 Mini Pumps left on them. After a long storage, verify the metering accuracy of the pumps.

For more information visit www.westsystem.com.au and www.atlcomposites.com.au

Related Articles

Resto brings legend back to life
A classic 32-foot Cayzer motor yacht built in 1976 is poised to return to the water A classic 32-foot Cayzer motor yacht built in 1976 is poised to return to the water as a one-of-a-kind gentleman's cruiser, thanks to the vision of its owner, the talents of the restoration team at Tasmanian Shipwrights & Co. and WEST SYSTEM products. Posted on 2 May
Upholding Tradition
West System and Epifanes bring a family treasure back to life Suspended in a cradle at the former Creese's yard, Battery Point, a 40-year-old 40-foot timber yacht is being brought back to its original form with the aim of competing in the 80th Rolex Sydney Hobart. Posted on 23 Apr
The future is strong with TechniGlue adhesives
Relied on by some of the world's most recognised boat builders ATL Composites is the reputable Australian formulator for a range of epoxy resin products, including the proven TECHNIGLUE high strength adhesives. Posted on 12 Apr
Schionning cat specifies DuFLEX panels
An expertly custom-crafted Schionning catamaran will sail the world with ease An expertly custom-crafted Schionning catamaran will sail the world with ease, thanks to the strong, durable DuFLEX Build System. Posted on 20 Mar
WEST SYSTEM is the go-to for all boat maintenance
Get your boat in top condition with the WEST SYSTEM range of epoxy products Get your boat in top condition with the WEST SYSTEM range of epoxy products which suit all kinds of vessels and maintenance projects involving aluminium, fibreglass, reinforcing fabrics, plastic, wood or composites. Posted on 5 Jan
Breiana Whitehead's Composite Collaboration
The quest to create the gold-medal-winning board with ATL Composites It's a long way from Townsville to Paris, and Australian Olympic kite-foiler, Breiana Whitehead is relying on a collaboration with ATL Composites to give her the winning edge in July 2024. Posted on 27 Dec 2023
METS opens with intense interest in composites
ATL in Australia supplies all the resin used in the panels made by vdL Composites On the first day of METSTRADE Show 2023, ATL Composites, Australia and their joint venture partners, von der Linden GmbH based in Wesel, Germany, exhibited the DuFLEX, DuraKore and Featherlight panels range Posted on 20 Nov 2023
Epifanes delivers the gloss and protection
Setting the standard in marine coatings since 1902 Adding to its complement of internationally respected and popular composite products, ATL Composites represents the EPIFANES range of Yacht Varnishes. Posted on 15 Nov 2023
Duratec Hi-Gloss Additive enhances gel coat
Spray your Gel Coat like paint and sand till it shines With over 30 years of successful use, Duratec Hi-Gloss Additive #904-001, is the proven leader for post-application gel coat work. Posted on 3 Nov 2023
ATL Composites heads to METS 2023
METSTRADE Show unites the world's leisure marine brands The METSTRADE Show in Amsterdam, 15 to 17 November 2023, unites the world's leisure marine brands and businesses in the world's largest B2B exhibition of marine equipment, systems and materials Posted on 28 Aug 2023